Average response time: under 24 hours

Restore 50-year-old terrazzo by grinding with coarse metal-bond segments to expose fresh chips, then polishing with resin pads from 100 up to 1500–3000 grit, finishing with a densifier or sealer. Work wet on terrazzo to protect the softer matrix.
| Stage | Pads | Grit |
|---|---|---|
| Expose chips | Metal bond | 30–50 |
| Transition | Hybrid / transitional | 100–200 |
| Polish | Resin | 400–800 |
| Gloss | Resin + wool | 1500–3000 |
A: Dry is possible but hotter and dustier; wet is safer for the matrix and gives better gloss on older floors.
A: Just enough to make chips flush — usually 1–2 passes with coarse metal. Too deep creates pitting that must be repaired.
A: Yes. Densify or seal to protect the matrix and make the gloss easier to maintain.
Restoring terrazzo is a grind-then-polish process. Expose chips with metal, polish with resin and wool, then protect the floor with a sealer. Start with terrazzo resin pads for consistent results.
كتبه وراجعه JOY TECH - مصنع أدوات الماس الحائز على تدقيق SGS وBV، والمعتمد CE/RoHS، والذي تأسس عام 2004 ويصدر إلى أكثر من 50 دولة.
مصنعنا ونظام إدارة الجودة لدينا يخضعان لتدقيق SGS وBureau Veritas. المنتجات تفي بمتطلبات CE/RoHS ويتم فحص كل قطعة بنسبة 100% قبل التعبئة.
Verified Certificates